Magnesia-Alumina Spinel Bricks
Itme |
Magnesia-Alumina Brick |
Magnesia-Alumina Spinel Bricks |
||
ML-80A |
ML-80B |
LMJ-80B |
LMJ-75B |
|
MgO,% |
≥ 80 |
≥ 80 |
≥ 80 |
≥ 75 |
Al 2 O 3 , % |
5~10 |
5~10 |
8~15 |
8~15 |
Apparent Porosity , % |
≤ 18 |
≤ 20 |
≤ 17 |
≤ 18 |
0.2 Mpa Refractoriness Under Load , ℃ |
≥ 1600 |
≥ 1580 |
≥ 1700 |
≥ 1650 |
Cold Crushing Strength , Mpa |
≥ 45 |
≥ 40 |
≥ 35 |
≥ 35 |
Thermal Shock Resistance (1100℃ , water) , cycle |
— |
≥ 20 |
≥ 15 |
|