MgO-AL2O3-Cr2O3 Brick
Brand |
LMLGe-75 |
LMLGe-80 |
MgO , % |
≥75 |
≥80 |
Cr 2 O 3 , % |
≥3 |
≥3 |
AL 2 O 3 , % |
≥7 |
≥7 |
Apparent Porosity (%) |
≤18 |
≤18 |
0.2MPa Refractoriness Under Load T0.6( o C) |
≥1650 |
≥1680 |
Cold Crushing Strength(MPa) |
≥35 |
≥40 |
Thermal shock resistance ( 1100 o C water- cooling) |
≥8 |
≥10 |